| ▲ | boppo1 3 hours ago | |||||||
I'm new to it and having trouble finding guides: - how do I apply it as a coating? I want it to be ~ 1/6" to 1/8" thick and as hard as possible - will turpentine dissolve or soften it? | ||||||||
| ▲ | chromacity 3 hours ago | parent | next [-] | |||||||
It's a relatively soft plastic and I don't think you can realistically build a uniform, good-looking layer that's 1/8" thick, if that's what you mean. If you need that thickness, high hardness, and nice appearance, I think your best bet is just a sheet of glass or acrylic on top. It can be used as protective varnish, but that would be a very thin layer, probably 0.1 mm or something like that. | ||||||||
| ||||||||
| ▲ | halestock 3 hours ago | parent | prev [-] | |||||||
I found a couple: https://resources.culturalheritage.org/osg-postprints/wp-con... https://www.zoicpaleotech.com/pages/paraloid-b72-in-fossil-p... acetone will dissolve it, dunno about turpentine. | ||||||||
| ||||||||